Private on-device repair evidence
Resin Print Not Sticking to the Build Plate
A detailed STLBEAST repair guide to restore bottom-layer adhesion without excessive exposure. Learn how to recognize the symptom, rank the likely causes, apply safe fixes in order, verify the result, and prevent the failure from returning.
Not started0 of 8 stepsNot yet saved

Record the setup that produced this result
Saved only in this browser with the repair. Nothing is uploaded.
Add before and after photos for this report
Photos stay in this open page only and are never stored or uploaded. They appear in the printed report while the page remains open.
Controlled test history
No controlled tests have been logged yet. Return to Workshop Mode and record each change before running another test.
Step completion
- 1Document the failure and confirm that it matches this guide: The raft remains in the vat or only part of the model attaches to the plate.Not completed
- 2Return extreme overrides to a known printer, nozzle, material, and slicer profile so the diagnosis starts from a stable baseline.Not completed
- 3Check build plate not leveled. Re-level the plate.Not completed
- 4Check bottom exposure too low. Clean it as specified.Not completed
- 5Inspect plate contamination. Use resin-tested bottom exposure.Not completed
- 6Rule out lift force too high. Reduce lift stress.Not completed
- 7Change only the single setting or hardware condition supported by the evidence, then run a small test that reproduces the original failure.Not completed
- 8Compare the test against the target condition, record the successful value, and save it in a printer/material profile before repeating the full print.Not completed
Observations and winning values
No notes recorded.
Verification test
- Model
- Small resin validation print
- Setup
- Use the final resin, temperature, exposure, lift and support profile.
- Pass
- The part completes with clean details, attached supports and no layer split.
- If unchanged
- The part detaches, splits, warps or loses detail.