Private on-device repair evidence
Nozzle Too Close to the Bed
Identify an over-squished first layer, scraping nozzle, blocked extrusion, ridges, and elephant-foot symptoms.
Not started0 of 6 stepsNot yet saved

Record the setup that produced this result
Saved only in this browser with the repair. Nothing is uploaded.
Add before and after photos for this report
Photos stay in this open page only and are never stored or uploaded. They appear in the printed report while the page remains open.
Controlled test history
No controlled tests have been logged yet. Return to Workshop Mode and record each change before running another test.
Step completion
- 1Stop the print if the nozzle is scraping the surface.Not completed
- 2Inspect the nozzle and plate for damage or debris.Not completed
- 3Raise Z offset in very small increments while running a first-layer pattern.Not completed
- 4Confirm the correct plate and mesh profile are active.Not completed
- 5Return first-layer flow to the validated profile before compensating with Z offset.Not completed
- 6Check that the nozzle is installed correctly and the hotend is mechanically secure.Not completed
Observations and winning values
No notes recorded.
Verification test
- Model
- Single-layer five-zone test
- Setup
- Use the final plate, material, mesh and first-layer profile.
- Pass
- Lines join evenly in the centre and corners, with no scraping, gaps or lifting.
- If unchanged
- One or more zones remain loose, transparent, ridged or detached.