Private on-device repair evidence
Support Scars and Rough Undersides
Improve surfaces above supports, reduce pitting, and protect visible detail.
Not started0 of 7 stepsNot yet saved

Record the setup that produced this result
Saved only in this browser with the repair. Nothing is uploaded.
Add before and after photos for this report
Photos stay in this open page only and are never stored or uploaded. They appear in the printed report while the page remains open.
Controlled test history
No controlled tests have been logged yet. Return to Workshop Mode and record each change before running another test.
Step completion
- 1Rotate the model to protect the most visible surface.Not completed
- 2Use painted/manual supports to limit contact to necessary areas.Not completed
- 3Tune top Z distance with a small sample.Not completed
- 4Use two or more interface layers at a sensible density when the slicer supports it.Not completed
- 5Slow the first layer above support.Not completed
- 6Tune cooling and bridge flow for the material.Not completed
- 7Consider splitting and joining the model.Not completed
Observations and winning values
No notes recorded.
Verification test
- Model
- Small overhang and support coupon
- Setup
- Use the final layer height, support interface and cooling profile.
- Pass
- Supports detach predictably and the underside is intact.
- If unchanged
- Supports fuse, collapse or leave severe scars.