HUB.STLBEAST3D PRINTING KNOWLEDGE HUB
FIRST LAYER DIAGNOSTIC

READ THE FIRST LAYER BEFORE CHANGING SETTINGS.

Use the visible shape of the line to separate nozzle height, surface contamination, temperature, flow and speed problems.

Z
OFFSET

Nozzle too high

Lines remain round, separate easily and leave gaps. Lower Z offset in very small steps after confirming the plate is clean.

Correct height

Adjacent lines touch with a smooth top and consistent width without a sharp ridge or transparent scraping.

Nozzle too low

Lines are overly transparent, ridged or scraped. Raise Z offset slightly and confirm flow is not excessive.

Fastest safe order

  1. Wash or clean the plate using the manufacturer-safe method.
  2. Confirm plate installation, mesh and mechanical stability.
  3. Adjust Z offset using a single-layer test.
  4. Only then change first-layer temperature or speed.

Common traps

  • Using flow to hide a bad Z offset.
  • Adding glue before cleaning contamination.
  • Changing mesh, temperature and speed together.
  • Ignoring a loose bed, nozzle or toolhead.